The Hot Corrosion of Fe-based Alloys with pre-coating NaCl/Na2SO4 Mixtures.
碩士 === 國立臺灣科技大學 === 機械工程系 === 87 === Abstract The high-temperature corrosion behavior of the three Fe base alloys, containing Fe-29.1Mn-8.98Al-0.75C (Fe-Mn-Al), STP-A26 alloy (A26), and 310 heat-resistant steel (310SS) has been studied at 750℃ in air with 2 mg/cm2 mixtures of various...
Main Authors: | Yong-Hua Su, 蘇永華 |
---|---|
Other Authors: | Chaur-Jeng Wang |
Format: | Others |
Language: | zh-TW |
Published: |
1999
|
Online Access: | http://ndltd.ncl.edu.tw/handle/80264970687324683189 |
Similar Items
-
The 3.5%NaCl Aqueous Corrosion of Fe-based Alloys After Hot Corrosion with pre-coating NaCl/Na2SO4 Mixtures
by: Ma, hsi-chang, et al.
Published: (2000) -
Hot Corrosion of Fe-Ni-Cr Alloys Caused by NaCl Deposits
by: Chien Shing Lin, et al.
Published: (1996) -
The high-temperature corrosion mechanism of Fe-Mn-Al-C alloy with NaCl coating
by: Chang Yeong-Chung, et al.
Published: (2002) -
The Hot Corrosion of Fe-base Alloys with NaCl / Na2SO4 Mixed Deposits in a Combustion Furnace
by: Jenq-Yih Pan, et al.
Published: (2004) -
Hot Corrosion of Co-based Alloys with 25%NaCl+75%Na2SO4 Coating at 1173 K
by: Fu Guangyan, et al.
Published: (2013-06-01)