The hot working characteristics of Al-0.65% Fe, and Al-0.5% Fe-0.5% Co conductor alloys

Recrystallized, rolled rods of the two conductor alloys were deformed in continuous torsion tests between 200 and 500C̕ and 0.02 and 5 s -1 , and in interrupted torsion tests at 400 and 450C̕, and 0.1 and 1.0 s -1 . The flow stresses were found to depend on the strain rate through a hyperbolic sine...

Full description

Bibliographic Details
Main Author: Conrod, Kevin
Format: Others
Published: 2000
Online Access:http://spectrum.library.concordia.ca/1123/1/MQ54324.pdf
Conrod, Kevin <http://spectrum.library.concordia.ca/view/creators/Conrod=3AKevin=3A=3A.html> (2000) The hot working characteristics of Al-0.65% Fe, and Al-0.5% Fe-0.5% Co conductor alloys. Masters thesis, Concordia University.