Purposeful modification of carbonate fillers for waterborne paints
In order to maximize the potential of Ukrainian carbonate deposits in composition of waterborne paints were studied properties and their possible for modification by mechanochemical activation in the presence of CH3Si(OH)2OK. Filtration coefficient, size of the effective specific surface, hydrophil...
Main Authors: | , |
---|---|
Format: | Article |
Language: | English |
Published: |
PC Technology Center
2015-04-01
|
Series: | Tehnologìčnij Audit ta Rezervi Virobnictva |
Subjects: | |
Online Access: | http://journals.uran.ua/tarp/article/view/40242 |
id |
doaj-f4d469712b0c4795841308aed8eb9eef |
---|---|
record_format |
Article |
spelling |
doaj-f4d469712b0c4795841308aed8eb9eef2020-11-25T02:52:55ZengPC Technology CenterTehnologìčnij Audit ta Rezervi Virobnictva2226-37802312-83722015-04-0124(22)91210.15587/2312-8372.2015.4024240242Purposeful modification of carbonate fillers for waterborne paintsВолодимир Олександрович Комаха0Валентин Анатолійович Свідерський1Kyiv National University of Trade and Economics, Kyoto 19, Kyiv, Ukraine, 02156National Technical University of Ukraine "Kyiv Polytechnic Institute", Peremohy 37, Kyiv, Ukraine, 03056In order to maximize the potential of Ukrainian carbonate deposits in composition of waterborne paints were studied properties and their possible for modification by mechanochemical activation in the presence of CH3Si(OH)2OK. Filtration coefficient, size of the effective specific surface, hydrophilic factor for initial and modified materials are determined during the work in the methodology of moistening research at leaking of polar and nonpolar liquids. Based on the data can be argued that the surface modification of carbonate by hydroalcoholic solution CH3Si(OH)2OK makes its surface less hydrophilic, increases dispersion, reduces the size of interparticle capillary, increases the effective surface area and will enhance the properties of the finished composite materials. Thus, investigations have shown that at filling of waterborne paints by carbonates of Ukrainian deposits is reasonable to conduct their preliminary mechanical activation using hydroalcoholic solution CH3Si(OH)2OK at a concentration of 0,5 % wt, because this treatment allows to bring the nature of carbonate surface to film former and improve moistening and distribution of the filler particles in the coating structure.http://journals.uran.ua/tarp/article/view/40242carbonate fillersurface areapolymerophilicitymodificationsurfactants |
collection |
DOAJ |
language |
English |
format |
Article |
sources |
DOAJ |
author |
Володимир Олександрович Комаха Валентин Анатолійович Свідерський |
spellingShingle |
Володимир Олександрович Комаха Валентин Анатолійович Свідерський Purposeful modification of carbonate fillers for waterborne paints Tehnologìčnij Audit ta Rezervi Virobnictva carbonate filler surface area polymerophilicity modification surfactants |
author_facet |
Володимир Олександрович Комаха Валентин Анатолійович Свідерський |
author_sort |
Володимир Олександрович Комаха |
title |
Purposeful modification of carbonate fillers for waterborne paints |
title_short |
Purposeful modification of carbonate fillers for waterborne paints |
title_full |
Purposeful modification of carbonate fillers for waterborne paints |
title_fullStr |
Purposeful modification of carbonate fillers for waterborne paints |
title_full_unstemmed |
Purposeful modification of carbonate fillers for waterborne paints |
title_sort |
purposeful modification of carbonate fillers for waterborne paints |
publisher |
PC Technology Center |
series |
Tehnologìčnij Audit ta Rezervi Virobnictva |
issn |
2226-3780 2312-8372 |
publishDate |
2015-04-01 |
description |
In order to maximize the potential of Ukrainian carbonate deposits in composition of waterborne paints were studied properties and their possible for modification by mechanochemical activation in the presence of CH3Si(OH)2OK.
Filtration coefficient, size of the effective specific surface, hydrophilic factor for initial and modified materials are determined during the work in the methodology of moistening research at leaking of polar and nonpolar liquids.
Based on the data can be argued that the surface modification of carbonate by hydroalcoholic solution CH3Si(OH)2OK makes its surface less hydrophilic, increases dispersion, reduces the size of interparticle capillary, increases the effective surface area and will enhance the properties of the finished composite materials.
Thus, investigations have shown that at filling of waterborne paints by carbonates of Ukrainian deposits is reasonable to conduct their preliminary mechanical activation using hydroalcoholic solution CH3Si(OH)2OK at a concentration of 0,5 % wt, because this treatment allows to bring the nature of carbonate surface to film former and improve moistening and distribution of the filler particles in the coating structure. |
topic |
carbonate filler surface area polymerophilicity modification surfactants |
url |
http://journals.uran.ua/tarp/article/view/40242 |
work_keys_str_mv |
AT volodimiroleksandrovičkomaha purposefulmodificationofcarbonatefillersforwaterbornepaints AT valentinanatolíjovičsvídersʹkij purposefulmodificationofcarbonatefillersforwaterbornepaints |
_version_ |
1724727777392852992 |