PHASE FORMATION IN NiTiAl10 POWDER MIXTURE DURING HEATING TO 1100 °C
In this paper the comparison of NiTiAl10 wt. % with the binary NiTi46 wt. % prepared by powder metallurgy was researched. The method of combustion synthesis was carried out under following conditions: sintering temperature of 800 °C and 1100 °C and heating rate approx. 300 °C.min-1. The addition of...
Main Authors: | Pavel Salvetr, Andrea Školáková, Pavel Novák, Dalibor Vojtěch |
---|---|
Format: | Article |
Language: | English |
Published: |
SciCell s.r.o.
2018-06-01
|
Series: | Acta Metallurgica Slovaca |
Subjects: | |
Online Access: | https://journals.scicell.org/index.php/AMS/article/view/267 |
Similar Items
-
Reactive Sintering Mechanism and Phase Formation in Ni-Ti-Al Powder Mixture During Heating
by: Pavel Salvetr, et al.
Published: (2018-04-01) -
Mechanism of the Intermediary Phase Formation in Ti-20 wt. % Al Mixture during Pressureless Reactive Sintering
by: Andrea Školáková, et al.
Published: (2019-07-01) -
High-Pressure Spark Plasma Sintering (HP SPS): A Promising and Reliable Method for Preparing Ti–Al–Si Alloys
by: Anna Knaislová, et al.
Published: (2017-04-01) -
Advanced Powder Metallurgy Technologies
by: Pavel Novák
Published: (2020-04-01) -
On Ti-18Si-6B and Ti-7.5Si-22.5B powder alloys prepared by high-energy ball milling and sintering
by: Bruno Bacci Fernandes, et al.
Published: (2012-12-01)