Modeling of the flow stress behavior and microstructural evolution during hot deformation of Mg–8Al–1.5Ca–0.2Sr magnesium alloy
Hot compression tests of Mg–8Al–1.5Ca–0.2Sr magnesium alloy were performed on the Gleeble-1500 machine at temperatures of 300, 350, 400, and 450 °C and strain rates of 0.01, 0.1 and 1 s−1. The flow stress behavior and microstructural evolution were followed. The work hardening was derived according...