Low Cycle Fatigue Behaviors of Single Crystal Nickel-based Superalloy at Temperatures of 600~760 <b>℃</b>
Low cycle fatigue (LCF) tests were conducted on a single crystal nickel-based superalloy DD6 with crystallographic orientations [001] at different elevated temperatures. The typical temperatures selected are 600 ℃, 650 ℃, 700 ℃ and 760 ℃, which represent the temperature field of turbine blade root o...
Main Authors: | ZHANG Zhihua, YU Huichen, LI Ying, DONG Chengli |
---|---|
Format: | Article |
Language: | zho |
Published: |
Journal of Aeronautical Materials
2018-06-01
|
Series: | Journal of Aeronautical Materials |
Subjects: | |
Online Access: | http://jam.biam.ac.cn/CN/Y2018/V38/I3/58 |
Similar Items
-
Low Cycle Fatigue of Single Crystal Nickel-based Superalloy DD6 at 1100℃
by: ZHANG Shichao, et al.
Published: (2018-02-01) -
Effects of check corrosion on high cycle fatigue properties of nickel-base single crystal superalloy
by: DONG Jian-min, et al.
Published: (2020-01-01) -
Orientation Dependence of High Cycle Fatigue Behavior of a <111> Oriented Single-Crystal Nickel-Based Superalloy
by: Bin Hu, et al.
Published: (2021-08-01) -
Low cycle fatigue properties and microstructure evolution at 760 °C of a single crystal superalloy
by: Zhenxue Shi, et al.
Published: (2015-02-01) -
Effect of different drilling techniques on high-cycle fatigue behavior of nickel-based single-crystal superalloy with film cooling hole
by: Zhang Zhijin, et al.
Published: (2021-04-01)