Thermal treatment of kaolin clay to obtain metakaolin
The metakaolin was produced by thermal treatment (calcination) of the starting high-quality kaolin clay from Serbia. The optimal calcination parameters, for which nearly complete dehydroxylation of the material was achieved, are: temperature 650°C and heating time of 90 min. The conversion of the ka...
Main Authors: | Ilić Biljana R., Mitrović Aleksandra A., Miličić Ljiljana R. |
---|---|
Format: | Article |
Language: | English |
Published: |
Association of Chemical Engineers of Serbia
2010-01-01
|
Series: | Hemijska Industrija |
Online Access: | http://www.doiserbia.nb.rs/img/doi/0367-598X/2010/0367-598X1000014I.pdf |
Similar Items
-
Research of possibilities for use domestic kaolin clays for production of metakaolin
by: Mitrović Aleksandra A., et al.
Published: (2009-01-01) -
Properties of Portland-Composite Cements with metakaolin: Commercial and manufactured by Thermal Activation of Serbian Kaolin Clay
by: Mitrovic A., et al.
Published: (2012-09-01) -
Mechanochemical treatment of Serbian kaolin clay to obtain high reactive pozzolana
by: Mitrović Aleksandra, et al.
Published: (2013-01-01) -
Evolution of Metakaolin Thermal and Chemical Activation from Natural Kaolin
by: Isabel Sánchez, et al.
Published: (2020-06-01) -
EFFECT OF KAOLIN ADDITION INTO METAKAOLIN GEOPOLYMER COMPOSITE
by: Alexey Manaenkov, et al.
Published: (2020-04-01)