Effect of MgO Addition on the Surface and Catalytic Properties of the CuO/AlO System

The effect of MgO on the solid–solid interactions, surface and catalytic properties of CuO/Al 2 O 3 solids was investigated using XRD methods, nitrogen adsorption at −196°C and oxidation of CO by O 2 at 150–300°C. The nominal composition of the pure mixed solid was 0.20CuO:Al 2 O 3 and the amounts o...

Full description

Bibliographic Details
Main Author: Nasr-Allah M. Deraz
Format: Article
Language:English
Published: Hindawi - SAGE Publishing 2001-03-01
Series:Adsorption Science & Technology
Online Access:https://doi.org/10.1260/0263617011494033
id doaj-e61ac2355af947c89d2ee912df5659d1
record_format Article
spelling doaj-e61ac2355af947c89d2ee912df5659d12021-04-02T16:54:08ZengHindawi - SAGE PublishingAdsorption Science & Technology0263-61742048-40382001-03-011910.1260/0263617011494033Effect of MgO Addition on the Surface and Catalytic Properties of the CuO/AlO SystemNasr-Allah M. DerazThe effect of MgO on the solid–solid interactions, surface and catalytic properties of CuO/Al 2 O 3 solids was investigated using XRD methods, nitrogen adsorption at −196°C and oxidation of CO by O 2 at 150–300°C. The nominal composition of the pure mixed solid was 0.20CuO:Al 2 O 3 and the amounts of MgO added varied between 0.43 wt% and 3.30 wt%. The pure and MgO-treated solids were subjected to precalcination (thermal treatment) at 600°C and 800°C, respectively. The results obtained revealed that CuO underwent solid–solid interactions with pure and doped alumina at temperatures of 600°C and above to yield a poorly crystalline copper aluminate (CuAl 2 O 4 ) phase. The amount of copper aluminate produced increased on increasing the precalcination temperature to 800°C. Magnesium oxide inhibited the formation of CuAl 2 O 4 at 600°C but enhanced this reaction at 800°C, the inhibiting and enhancing effects depending on the amount of MgO present. Doping with MgO effected a measurable increase in both the specific surface areas and catalytic activities of the solids precalcined at 600°C. The reverse effect was observed for the doped solids preheated in air at 800°C. Doping at 600°C and 800°C modified the concentration of catalytically active constituents involved in chemisorption and catalysis of the CO oxidation reaction.https://doi.org/10.1260/0263617011494033
collection DOAJ
language English
format Article
sources DOAJ
author Nasr-Allah M. Deraz
spellingShingle Nasr-Allah M. Deraz
Effect of MgO Addition on the Surface and Catalytic Properties of the CuO/AlO System
Adsorption Science & Technology
author_facet Nasr-Allah M. Deraz
author_sort Nasr-Allah M. Deraz
title Effect of MgO Addition on the Surface and Catalytic Properties of the CuO/AlO System
title_short Effect of MgO Addition on the Surface and Catalytic Properties of the CuO/AlO System
title_full Effect of MgO Addition on the Surface and Catalytic Properties of the CuO/AlO System
title_fullStr Effect of MgO Addition on the Surface and Catalytic Properties of the CuO/AlO System
title_full_unstemmed Effect of MgO Addition on the Surface and Catalytic Properties of the CuO/AlO System
title_sort effect of mgo addition on the surface and catalytic properties of the cuo/alo system
publisher Hindawi - SAGE Publishing
series Adsorption Science & Technology
issn 0263-6174
2048-4038
publishDate 2001-03-01
description The effect of MgO on the solid–solid interactions, surface and catalytic properties of CuO/Al 2 O 3 solids was investigated using XRD methods, nitrogen adsorption at −196°C and oxidation of CO by O 2 at 150–300°C. The nominal composition of the pure mixed solid was 0.20CuO:Al 2 O 3 and the amounts of MgO added varied between 0.43 wt% and 3.30 wt%. The pure and MgO-treated solids were subjected to precalcination (thermal treatment) at 600°C and 800°C, respectively. The results obtained revealed that CuO underwent solid–solid interactions with pure and doped alumina at temperatures of 600°C and above to yield a poorly crystalline copper aluminate (CuAl 2 O 4 ) phase. The amount of copper aluminate produced increased on increasing the precalcination temperature to 800°C. Magnesium oxide inhibited the formation of CuAl 2 O 4 at 600°C but enhanced this reaction at 800°C, the inhibiting and enhancing effects depending on the amount of MgO present. Doping with MgO effected a measurable increase in both the specific surface areas and catalytic activities of the solids precalcined at 600°C. The reverse effect was observed for the doped solids preheated in air at 800°C. Doping at 600°C and 800°C modified the concentration of catalytically active constituents involved in chemisorption and catalysis of the CO oxidation reaction.
url https://doi.org/10.1260/0263617011494033
work_keys_str_mv AT nasrallahmderaz effectofmgoadditiononthesurfaceandcatalyticpropertiesofthecuoalosystem
_version_ 1721555108364288000