Defect “steel-melting captivity and swelling” on the inner surface of seamless hot-rolled pipes. Characteristic genetic features, the causes of formation and measures of prevention.
In a market economy, increasing the competitiveness of steel products is an urgent trend in science and practice. Development of production of new pipe steels in terms of pipe-rolling plant open joint-stock company «BSW – management company of holding «Belarusian metallurgical company» casted on con...
Main Authors: | I. A. Kovaleva, N. A. Khodosovskaya |
---|---|
Format: | Article |
Language: | English |
Published: |
Belarusian National Technical University
2020-01-01
|
Series: | Litʹë i Metallurgiâ |
Subjects: | |
Online Access: | https://lim.bntu.by/jour/article/view/3152 |
Similar Items
-
Predicting Susceptibility to Solidification Cracking and Liquation Cracking by CALPHAD
by: Sindo Kou
Published: (2021-09-01) -
Friction Stir Processing Nickel-Base Alloys
by: Rule, James R.
Published: (2011) -
Separation and coalescence phenomena in three phase systems
by: Smith, Peter Graham.
Published: (1984) -
Liquation Cracking Tendency of Novel Al-Mg-Zn Alloys with a Zn/Mg Ratio below 1.0 during Fusion Welding
by: Di Zhang, et al.
Published: (2020-02-01) -
Effects of surface active agents on drop size in liquid-liquid systems
by: Slaymaker, Elizabeth Ann
Published: (2006)