Chemical Degradation of PSF-PUR Blend Hollow Fiber Membranes—Assessment of Changes in Properties and Morphology after Hydrolysis
In this study, we focused on obtaining polysulfone-polyurethane (PSF-PUR) blend partly degradable hollow fiber membranes (HFMs) with different compositions while maintaining a constant PSF:PUR = 8:2 weight ratio. It was carried out through hydrolysis, and evaluation of the properties and morphology...
Main Authors: | Wioleta Sikorska, Monika Wasyłeczko, Małgorzata Przytulska, Cezary Wojciechowski, Gabriel Rokicki, Andrzej Chwojnowski |
---|---|
Format: | Article |
Language: | English |
Published: |
MDPI AG
2021-01-01
|
Series: | Membranes |
Subjects: | |
Online Access: | https://www.mdpi.com/2077-0375/11/1/51 |
Similar Items
-
Biodegradation Process of PSF-PUR Blend Hollow Fiber Membranes Using <i>Escherichia coli </i>Bacteria—Evaluation of Changes in Properties and Porosity
by: Wioleta Sikorska, et al.
Published: (2021-04-01) -
On the crack path under mixed mode loading on PUR foams
by: L. Marsavina, et al.
Published: (2015-09-01) -
The influence of adhesive joint characteristics of the bonded samples of PUR-foam
by: Josef Pacovský
Published: (2011-01-01) -
On the crack path under mixed mode loading on PUR foams
by: L. Marsavina, et al.
Published: (2015-10-01) -
Life cycle cost analysis -With focus on the floor types, linoleum and vinyl with or without PUR reinforced surface
by: Miletic, Martin, et al.
Published: (2014)