STRUCTURE AND OPTICAL PROPERTIES OF CdSe THIN FILMS AS A FUNCTION OF THE ANNEALING TIME
Cadmium (Cd) and selenide powder used to prepared cadmium selenide alloy. (CdSe) thin films of thickness 1320 Å were thermally evaporated technique deposited on glass substrate at room temperature. The as-deposited films were annealed in air atmosphere at 100oC, for three different annealing times (...
Main Author: | Eman M. Noori |
---|---|
Format: | Article |
Language: | Arabic |
Published: |
Al-Mustansiriyah University
2017-07-01
|
Series: | Mustansiriyah Journal of Science |
Subjects: | |
Online Access: | http://mjs.uomustansiriyah.edu.iq/ojs1/index.php/MJS/article/view/175 |
Similar Items
-
Chemical synthesis and characterization of CdSe thin films deposited by SILAR technique for optoelectronic applications
by: K.B. Chaudhari, et al.
Published: (2016-12-01) -
Molecular dynamics simulations of the elastic properties of CdSe nanowires
by: CHEN Na, et al.
Published: (2012-12-01) -
A mechanistic study of the electrochemical formation of CdS CdSe semiconducting films
by: Aparicio-Razo, Mario
Published: (1983) -
Photoluminescent properties of annealed ZnCdSe epitaxial layers on InP substrates =: 磷化銦上鋅鎘硒外延層退火處理後的光致發光性質.
Published: (1998) -
Photoinduced transformations of optical properties of CdSe and Ag-In-S nanocrystals embedded in the films of polyvinyl alcohol
by: Tetyana Kryshtab, et al.
Published: (2016-06-01)