Microstructural path of recrystallization in a commercial Al-Mn-Fe-Si (AA3003) alloy

The phenomenological analysis of recrystallization data is described. The concept of microstructural path is briefly introduced as well as some of its relevant equations. The correct equation for the impingement compensated chord length is introduced and used here for the first time. The theory is t...

Full description

Bibliographic Details
Main Authors: Paulo Rangel Rios, Angelo Fernando Padilha
Format: Article
Language:English
Published: Associação Brasileira de Metalurgia e Materiais (ABM); Associação Brasileira de Cerâmica (ABC); Associação Brasileira de Polímeros (ABPol) 2003-12-01
Series:Materials Research
Subjects:
Online Access:http://www.scielo.br/scielo.php?script=sci_arttext&pid=S1516-14392003000400030
Description
Summary:The phenomenological analysis of recrystallization data is described. The concept of microstructural path is briefly introduced as well as some of its relevant equations. The correct equation for the impingement compensated chord length is introduced and used here for the first time. The theory is then applied to data from the recrystallization of a commercial Al-Mn-Fe-Si (AA3003) alloy. It is concluded that nucleation is site saturated and that the grain boundary velocity decreases with time. The analysis also shows that the shape of the recrystallized regions significantly deviates from spherical as the reaction progresses, probably because of the boundary/precipitates interaction.