Low temperature production of wollastonite from limestone and silica sand through solid-state reaction
Wollastonite was produced using solid-state reaction from limestone and silica sand. Limestone containing a high percentage of CaO (55.10%) and silica sand with 99% SiO2 were used as starting materials. The ratios of limestone/sand used were 1:1, 2:1 and 3:1 with various firing temperatures, namely...
Main Authors: | Rashita Abd Rashid, Roslinda Shamsudin, Muhammad Azmi Abdul Hamid, Azman Jalar |
---|---|
Format: | Article |
Language: | English |
Published: |
Taylor & Francis Group
2014-03-01
|
Series: | Journal of Asian Ceramic Societies |
Subjects: | |
Online Access: | http://www.sciencedirect.com/science/article/pii/S2187076414000190 |
Similar Items
-
Bioactivity and Cell Compatibility of β-Wollastonite Derived from Rice Husk Ash and Limestone
by: Roslinda Shamsudin, et al.
Published: (2017-10-01) -
SINTESIS DAN KARAKTERISASI WOLLASTONIT BERBAHAN DASAR ALAMI DENGAN METODE HIDROTERMAL
by: Rianda -, et al.
Published: (2015-03-01) -
Prospect of Metal Ceramic (Titanium-Wollastonite) Composite as Permanent Bone Implants: A Narrative Review
by: Lohashenpahan Shanmuganantha, et al.
Published: (2021-01-01) -
Effects of Heat-Treatment and Nano-Wollastonite Impregnation on Fire Properties of Solid Wood
by: Abolfazl Soltani, et al.
Published: (2016-09-01) -
Defects and Calcium Diffusion in Wollastonite
by: Sumudu Nimasha, et al.
Published: (2020-11-01)