Effect of Zr Additions on Non-Metallic Inclusions in X11CrNiMo12 Steel
The production of clean steel is associated with high-quality steel grades for demanding applications. The formation of oxide inclusions mainly depends on the deoxidation practice; it is usually carried out through Al additions, but alumina inclusions can have detrimental effects. An alternative zir...
Main Authors: | Jaka Burja, Mitja Koležnik, Barbara Šetina Batič, Jožef Medved |
---|---|
Format: | Article |
Language: | English |
Published: |
MDPI AG
2020-09-01
|
Series: | Metals |
Subjects: | |
Online Access: | https://www.mdpi.com/2075-4701/10/9/1183 |
Similar Items
-
Development of banded microstructure in 34CrNiMo6 steel
by: A. Nagode, et al.
Published: (2016-07-01) -
Microstructure and Tribological Properties of Laser Forming Repaired 34CrNiMo6 Steel
by: Chunping Huang, et al.
Published: (2018-09-01) -
Impact strength of GX8CrNi12, GX5CrNi18-9 and GX5CrNiMo19-11-2 cast steel at - 30 °C
by: B. Kalandyk, et al.
Published: (2016-10-01) -
Microstructure features of 24CrNiMo alloy steel fabricated by laser additive manufacturing
by: XU Yun-hua, et al.
Published: (2020-11-01) -
Microstructure and mechanical properties of 34CrNiMo6 steel repaired by laser remelting
by: Renyu Liang, et al.
Published: (2020-11-01)