Cold drawing schedules for RSt 34-2 (1.0034) steel wire for correction of overheating defects and breakless ensuring
The paper’s authors researched the defects correction for RSt 34-2 (1.0034) steel wire, obtained as result of its overheating at 1140...1160 °C. Instead of the re-heat treatment method, the authors proposed five cold drawing, annealing and overheating combination schedules, which ensure the increase...
Main Authors: | Anishchenko Oleksandr, Kukhar Volodymyr, Oginskiy Iosyp, Korenko Maryna, Prysiazhnyi Andrii |
---|---|
Format: | Article |
Language: | English |
Published: |
EDP Sciences
2021-01-01
|
Series: | E3S Web of Conferences |
Online Access: | https://www.e3s-conferences.org/articles/e3sconf/pdf/2021/60/e3sconf_tpacee2021_06005.pdf |
Similar Items
-
Stub Record for Image YMCA_0034.tif
Published: () -
Developing of X65 steel coils making at Steckel mill using thermo-mechanical control process
by: Kurpe Oleksandr, et al.
Published: (2021-01-01) -
Pyrazole compound BPR1P0034 with potent and selective anti-influenza virus activity
by: Yeh Jiann-Yih, et al.
Published: (2010-02-01) -
RHeSumaRST: um sumarizador automático de estruturas RST.
by: Seno, Eloize Rossi Marques
Published: (2016) -
Analysis of relation between edging ratio and deformation work done in pre-forming of workpiece by bulk buckling
by: Kukhar Volodymyr, et al.
Published: (2018-01-01)