Preculiarities in the Crystallization of Iron Containing up to 2.0 wt% of Carbon
Main Authors: | Siderov, V.E., Son, L.D., Rusakov, G.M., Baum, B.A. |
---|---|
Format: | Article |
Language: | English |
Published: |
De Gruyter
1995-10-01
|
Series: | High Temperature Materials and Processes |
Online Access: | https://doi.org/10.1515/HTMP.1995.14.4.263 |
Similar Items
-
The stress and temperature dependence of creep in an Al-2.0wt%Li alloy
by: Goodson, Earl F.
Published: (2013) -
The Properties of Composite Solders of Sn-3.0 wt.% Ag- 0.5 wt.% Cu alloy Added with Sn-10.0 wt.% Cu alloy
by: Chia-Yu Liu, et al.
Published: (2019) -
Correlation of Thermal and Microstructural Properties of an Al-0.60wt%Mg-0.25wt%Fe-0.05wt%Cu Alloy Unidirectionally Solidified
by: Pedro LAMARÃO, et al.
Published: (2014-09-01) -
Investigations on Microstructure and Properties of 16 wt% Cr-3 wt% B-0.6 wt% C-1 wt% Mn-Fe Alloy
by: Jiawei Ding, et al.
Published: (2018-07-01) -
Electromigration study of Sn-3wt.%Ag-0.5wt.%Cu-(3~10wt.%)Bi solders
by: Shang-Hua Lee, et al.
Published: (2011)