Preparation of hot-rolled potassium doped tungsten (KW) thick plate and performance of KW-Cu monoblock mock-ups under high heat flux testing
A 10-kg thick potassium doped tungsten (KW) plate with 70% deformation was prepared by hot rolling. After annealing (1800 °C, 1 h), the typical dovetail splicing morphology was formed which was related to the clustered potassium bubbles in the matrix. Both the as-received KW and annealed KW had the...