Debye’s temperature and heat capacity for Sr0.15Ba0.85Bi2Nb2O9 relaxor ferroelectric ceramic
A lead-free relaxor ferroelectric, Sr0.15Ba0.85Bi2Nb2O9, was synthesized via solid-state reaction and the temperature-dependence of the heat capacity was measured in a wide temperature range. The dielectric permittivity was also measured between 500Hz and 5MHz in the same temperature range. No anoma...
Main Authors: | A. Peláiz-Barranco, Y. González-Abreu, P. Saint-Grégoire, J. D. S. Guerra, F. Calderón-Piñar |
---|---|
Format: | Article |
Language: | English |
Published: |
World Scientific Publishing
2016-03-01
|
Series: | Journal of Advanced Dielectrics |
Subjects: | |
Online Access: | http://www.worldscientific.com/doi/pdf/10.1142/S2010135X16200010 |
Similar Items
-
Crossover from normal to diffused and relaxor ferroelectric in BaZrO3-modified (Ba0.85Ca0.15)TiO3 ceramics
by: Shao Bo Chen, et al.
Published: (2021-09-01) -
Electrocaloric effect and freezing temperature in (Pb0.8Ba0.2)[(Zn1∕3Nb2∕3)0.7Ti0.3]O3 relaxor ferroelectric ceramic
by: A. Peláiz-Barranco, et al.
Published: (2016-09-01) -
Structural and ferroelectric properties of Sr1−xBaxBi2Nb2O9 thin films obtained by dip-coating
by: Y. González-Abreu, et al.
Published: (2017-10-01) -
Relaxor ferroelectric behavior: An approach considering both the dipolar and electrical conductivity contributions
by: C. Carreras-Casas, et al.
Published: (2021-06-01) -
NMR and the local structure of relaxors
by: Blinc R., et al.
Published: (2002-01-01)