Processing of spent NiW/Al2O3 catalysts
Spent oxidized (500 ºC, 5 h) commercial NiW/Al2O3 catalysts were processed using two different routes: a) fusion with NaOH (650 ºC, 1 h), the roasted mass was leached in water; b) leaching with HCl or H2SO4 (70 ºC, 1-3 h). HCl was the best leachant. In both routes, soluble tungsten was extracted at...