Processing of spent NiW/Al2O3 catalysts

Spent oxidized (500 ºC, 5 h) commercial NiW/Al2O3 catalysts were processed using two different routes: a) fusion with NaOH (650 ºC, 1 h), the roasted mass was leached in water; b) leaching with HCl or H2SO4 (70 ºC, 1-3 h). HCl was the best leachant. In both routes, soluble tungsten was extracted at...

Full description

Bibliographic Details
Main Authors: Jéssica Frontino Paulino, Julio Carlos Afonso, José Waldemar Silva Dias da Cunha
Format: Article
Language:English
Published: Sociedade Brasileira de Química 2013-01-01
Series:Química Nova
Subjects:
Online Access:http://www.scielo.br/scielo.php?script=sci_arttext&pid=S0100-40422013000500016&lng=en&tlng=en