Penelitian mutu kulit sarung tangan golf samak krom
The Study aimed at improving the quality of chrome-tanned leather for golf floves producted by Indonesian tanners. Samples used in this study were 32. They were visually inspected and tested on their chemical and physical properties. The results of the chemical and physical tests were analyzed using...
Main Authors: | , , , |
---|---|
Format: | Article |
Language: | English |
Published: |
Center for Leather, Rubber, and Plastics
1992-12-01
|
Series: | Majalah Kulit, Karet, dan Plastik |
Online Access: | http://ejournal.kemenperin.go.id/mkkp/article/view/493/469 |
id |
doaj-afb854e495b74e70b08e721f01fc30cd |
---|---|
record_format |
Article |
spelling |
doaj-afb854e495b74e70b08e721f01fc30cd2020-11-25T01:38:29ZengCenter for Leather, Rubber, and PlasticsMajalah Kulit, Karet, dan Plastik1829-69712460-44611992-12-018151910.20543/mkkp.v8i15.493Penelitian mutu kulit sarung tangan golf samak kromSri Untari0Emiliana Kasmudjiastuti1Isti M2Wahyu Bintoro3Balai Besar Kulit, Karet, dan PlastikBalai Besar Kulit, Karet, dan PlastikBalai Besar Kulit, Karet, dan PlastikBalai Besar Kulit, Karet, dan PlastikThe Study aimed at improving the quality of chrome-tanned leather for golf floves producted by Indonesian tanners. Samples used in this study were 32. They were visually inspected and tested on their chemical and physical properties. The results of the chemical and physical tests were analyzed using deviation standard in descriptive statistics. It was obtained from the visual inspection of the samples taken that the leather was soft enough, the colour was even, their hair was not loose, and it was flexible but not elastic. While from the Chemical Tests, the results obtained were : water content (13,78 – 16,94) %; Fat Content (6,04 – 11,38) % and pH Valueness (4,43 – 5,19). It was obtained from the physical tests that Thickness (0,32 – 0,64) mm; well tanned; Tensile Strength resistence (106,07 – 109,73) kg/cm2; Flexibility (53,11 – 103,07) %; Slit Tear Resistance (13,48 – 39,22) kgf/cm; Stitch Tear Strength (74,51 – 137,79) kgf/cm, wet rub fastness tst shown a little discolourisation while dry rub fastness test shown no discolourisation.http://ejournal.kemenperin.go.id/mkkp/article/view/493/469 |
collection |
DOAJ |
language |
English |
format |
Article |
sources |
DOAJ |
author |
Sri Untari Emiliana Kasmudjiastuti Isti M Wahyu Bintoro |
spellingShingle |
Sri Untari Emiliana Kasmudjiastuti Isti M Wahyu Bintoro Penelitian mutu kulit sarung tangan golf samak krom Majalah Kulit, Karet, dan Plastik |
author_facet |
Sri Untari Emiliana Kasmudjiastuti Isti M Wahyu Bintoro |
author_sort |
Sri Untari |
title |
Penelitian mutu kulit sarung tangan golf samak krom |
title_short |
Penelitian mutu kulit sarung tangan golf samak krom |
title_full |
Penelitian mutu kulit sarung tangan golf samak krom |
title_fullStr |
Penelitian mutu kulit sarung tangan golf samak krom |
title_full_unstemmed |
Penelitian mutu kulit sarung tangan golf samak krom |
title_sort |
penelitian mutu kulit sarung tangan golf samak krom |
publisher |
Center for Leather, Rubber, and Plastics |
series |
Majalah Kulit, Karet, dan Plastik |
issn |
1829-6971 2460-4461 |
publishDate |
1992-12-01 |
description |
The Study aimed at improving the quality of chrome-tanned leather for golf floves producted by Indonesian tanners. Samples used in this study were 32. They were visually inspected and tested on their chemical and physical properties. The results of the chemical and physical tests were analyzed using deviation standard in descriptive statistics. It was obtained from the visual inspection of the samples taken that the leather was soft enough, the colour was even, their hair was not loose, and it was flexible but not elastic. While from the Chemical Tests, the results obtained were : water content (13,78 – 16,94) %; Fat Content (6,04 – 11,38) % and pH Valueness (4,43 – 5,19). It was obtained from the physical tests that Thickness (0,32 – 0,64) mm; well tanned; Tensile Strength resistence (106,07 – 109,73) kg/cm2; Flexibility (53,11 – 103,07) %; Slit Tear Resistance (13,48 – 39,22) kgf/cm; Stitch Tear Strength (74,51 – 137,79) kgf/cm, wet rub fastness tst shown a little discolourisation while dry rub fastness test shown no discolourisation. |
url |
http://ejournal.kemenperin.go.id/mkkp/article/view/493/469 |
work_keys_str_mv |
AT sriuntari penelitianmutukulitsarungtangangolfsamakkrom AT emilianakasmudjiastuti penelitianmutukulitsarungtangangolfsamakkrom AT istim penelitianmutukulitsarungtangangolfsamakkrom AT wahyubintoro penelitianmutukulitsarungtangangolfsamakkrom |
_version_ |
1725053506807660544 |