The fracture behavior transitions in cold dwell fatigue of Ti-6Al-4V
Ti-6Al-4V forged materials which had fine grain size and commercial billet which had moderate grain size and micro texture were prepared. Cold dwell fatigue tests were conducted using both materials, and dwell time condition was up to 1800s. Fracture cycles and elongation were almost same on each sp...
Main Authors: | Ozaki Tomomichi, Ota Yutaro, Kubushiro Keiji, Sano Kokichi |
---|---|
Format: | Article |
Language: | English |
Published: |
EDP Sciences
2020-01-01
|
Series: | MATEC Web of Conferences |
Online Access: | https://www.matec-conferences.org/articles/matecconf/pdf/2020/17/matecconf_ti2019_11085.pdf |
Similar Items
-
The rupture life prediction in cold dwell fatigue of Ti-6Al-4V based on the creep deformation
by: Ota Yutaro, et al.
Published: (2020-01-01) -
Mechanics and micro-mechanisms of LCF and dwell fatigue in Ti-6Al-4V
by: Tympel, Peter
Published: (2016) -
Elucidating the Role of Microstructure, Texture, and Microtexture on the Dwell Fatigue Response of Ti-6Al-4V
by: Blankenship, Alec Mitchell
Published: (2016) -
Data of dynamic microscale strain distributions of Ti-6Al-4V alloys in dwell fatigue tests
by: Qinghua Wang, et al.
Published: (2019-08-01) -
Fracture mechanics based fatigue and fracture toughness evaluation of SLM Ti-6Al-4V
by: Dhansay, Nur Mohamed
Published: (2017)