The porosity study of sintered products from electro-erosive materials of alloy Cr13, obtained in butyl alcohol

The article presents the results of a study of the porosity of sintered products from alloy X13 electroerosive materials obtained in butyl alcohol. It is shown that when hardening electroerosive materials from alloy X13 by the method of spark plasma sintering, the porosity was 3.347%.

Bibliographic Details
Main Authors: Khardikov S.V., Novikov A.N., Ageeva A.E.
Format: Article
Language:English
Published: EDP Sciences 2020-01-01
Series:MATEC Web of Conferences
Online Access:https://www.matec-conferences.org/articles/matecconf/pdf/2020/25/matecconf_icmtmte2020_02020.pdf
Description
Summary:The article presents the results of a study of the porosity of sintered products from alloy X13 electroerosive materials obtained in butyl alcohol. It is shown that when hardening electroerosive materials from alloy X13 by the method of spark plasma sintering, the porosity was 3.347%.