Cavity Behavior of Fine-Grained 5A70 Aluminum Alloy during Superplastic Formation

The study of the exact physical mechanism of cavity nucleation and growth is significant in terms of predicting the extent of internal damage following superplastic deformation. The 5A70 alloy was processed by cold rolling for 14 passes with a total reduction deformation of 90% (20⁻2 mm) a...

Full description

Bibliographic Details
Main Authors: Sheng Li, Shunyao Jin, Zhongguo Huang
Format: Article
Language:English
Published: MDPI AG 2018-12-01
Series:Metals
Subjects:
Online Access:https://www.mdpi.com/2075-4701/8/12/1065