Determination of Energy Characteristic and Microporous Volume by Immersion Calorimetry in Carbon Monoliths

Activated carbon monoliths disc and honeycomb type were prepared by chemical activation of coconut shell with zinc chloride at different concentrations, without using a binder. The structures were characterized by N2 adsorption at 77 K and immersion calorimetry into benzene. The experimental results...

Full description

Bibliographic Details
Main Authors: Juan Carlos Moreno-Piraján, Liliana Giraldo, Diana P. Vargas
Format: Article
Language:English
Published: Hindawi Limited 2012-01-01
Series:E-Journal of Chemistry
Online Access:http://dx.doi.org/10.1155/2012/976275
Description
Summary:Activated carbon monoliths disc and honeycomb type were prepared by chemical activation of coconut shell with zinc chloride at different concentrations, without using a binder. The structures were characterized by N2 adsorption at 77 K and immersion calorimetry into benzene. The experimental results showed that the activation with zinc chloride produces a wide microporous development, with micropore volume between 0,38 and 0,79 cm3g-1, apparent BET surface area between 725 and 1523 m2g-1 and immersion enthalpy between 73,5 and 164,2 Jg-1. We compared the experimental enthalpy with calculated enthalpy by equation Stoeckli-Kraehenbuehl finding a data dispersion from which can infer that the structures are not purely microporous; this fact is ratified with similar behavior that the evidence t the product EoWo.