Joining of Dissimilar Alloys Ti-6Al-4V and Ti-6Al-2Sn-4Zr-2Mo-0.1Si Using Linear Friction Welding
Dissimilar joints between Ti-6Al-4V (Ti-64) and Ti-6Al-2Sn-4Zr-2Mo-0.1Si (Ti-6242) were manufactured using linear friction welding. The weld quality, in terms of the microstructure and mechanical properties, was investigated after stress relief annealing (SRA) at 750 °C for 2 h and compared with the...
Main Authors: | , , , |
---|---|
Format: | Article |
Language: | English |
Published: |
MDPI AG
2020-08-01
|
Series: | Materials |
Subjects: | |
Online Access: | https://www.mdpi.com/1996-1944/13/17/3664 |