The effect of hydrogen gas evolution of magnesium implant on the postimplantation mortality of rats
Background/Objective: Hydrogen gas cavity is formed during in vivo degradation of magnesium implants. In many studies, the gas cavity is mostly punctured out subcutaneously. However, this procedure becomes inapplicable in certain internal surgeries; therefore, the effect of this gas cavity is worth...
Main Authors: | Deni Noviana, Devi Paramitha, Mokhamad Fakhrul Ulum, Hendra Hermawan |
---|---|
Format: | Article |
Language: | English |
Published: |
Elsevier
2016-04-01
|
Series: | Journal of Orthopaedic Translation |
Subjects: | |
Online Access: | http://www.sciencedirect.com/science/article/pii/S2214031X15000601 |
Similar Items
-
In-Vivo Corrosion Characterization and Assessment of Absorbable Metal Implants
by: Mokhamad Fakhrul Ulum, et al.
Published: (2019-04-01) -
Effect of Magnesium Fluoride on Hydrogenation Properties of Magnesium Hydride
by: Pragya Jain, et al.
Published: (2015-11-01) -
A Physical Approach to Simulate the Corrosion of Ceramic-Coated Magnesium Implants
by: Moataz Abdalla, et al.
Published: (2021-07-01) -
Biodegradable Magnesium Implants for Medical Applications
by: Tiasha, Tarannum R.
Published: (2017) -
Resistance of Magnesium Alloys to Corrosion Fatigue for Biodegradable Implant Applications: Current Status and Challenges
by: R. K. Singh Raman, et al.
Published: (2017-11-01)