Preparation and Properties of Superamphiphobic Wear-resistance PPS-based Coating
Superamphiphobic wear-resistance PPS-based coatings were prepared by a simple spraying method with a pore-forming reagent of NH<sub>4</sub>HCO<sub>3</sub> and nano-filler of carbon nanotubes (CNTs).The surface morphology and the hydrophobicity,oleophobicity of the coating wer...
Main Authors: | , , , |
---|---|
Format: | Article |
Language: | zho |
Published: |
Journal of Materials Engineering
2017-01-01
|
Series: | Journal of Materials Engineering |
Subjects: | |
Online Access: | http://jme.biam.ac.cn/CN/Y2017/V45/I1/38 |
Summary: | Superamphiphobic wear-resistance PPS-based coatings were prepared by a simple spraying method with a pore-forming reagent of NH<sub>4</sub>HCO<sub>3</sub> and nano-filler of carbon nanotubes (CNTs).The surface morphology and the hydrophobicity,oleophobicity of the coating were analyzed by scanning electron microscope (SEM) and contact angle meter.The wear-resistance of the coating was verified by sanding method with given load.The results indicate that a rough surface is obtained after pore-forming,and the porous structures in combination with the CNTs construct the special micro/nano-scale network structures.When the mass fraction of NH<sub>4</sub>HCO<sub>3</sub> is 5%,the contact angles of the coating for water,glycerine and ethylene glycol are 162°,158° and 152°,showing superamphiphobic property.After polished 10000 times by abrasive paper,the coating shows slight friction marks and remains high hydrophobicity,exhibiting excellent wear-resistance. |
---|---|
ISSN: | 1001-4381 1001-4381 |