Ex Situ Examination of Matrix and Inclusions of API-X100 before and after Exposure to Bitumen at Elevated Temperature
The corrosivity of bitumen at 60 and 120 °C was examined by exposing American Petroleum Institute (API) X100 (yield strength 100 ksi, 690 MPa) pipeline steel to bitumen in an autoclave for 30 days. Prior to the autoclave measurements, the inclusion types in the API-X100 pipeline steel were character...
Main Authors: | Hongxing Liang, Edouard Asselin |
---|---|
Format: | Article |
Language: | English |
Published: |
MDPI AG
2021-09-01
|
Series: | Materials |
Subjects: | |
Online Access: | https://www.mdpi.com/1996-1944/14/17/5007 |
Similar Items
-
PROBLEMS AND PROSPECTS OF PETROLEUM BITUMEN PRODUCTION
by: N. A. Belova, et al.
Published: (2016-07-01) -
Three phase corrosion of pipeline steel: Size effects of deposited solids under water droplets and an oil diffusion barrier
by: Hongxing Liang, et al.
Published: (2021-03-01) -
The bitumen batching system's modernization and its effective analysis at the asphalt mixing plant
by: Justas Bražiūnas, et al.
Published: (2010-09-01) -
Effects of Filler–Bitumen Ratio and Mineral Filler Characteristics on the Low-Temperature Performance of Bitumen Mastics
by: Chuanfeng Zheng, et al.
Published: (2018-07-01) -
ADDITIVES TO BITUMENS
by: N. A. Belova, et al.