Temperature threshold and water role in CVD growth of single-walled carbon nanotubes
An in-depth understanding of the growth process of single walled carbon nanotubes is of vital importance to the control of the yield of the material and its carbon structure. Using a nickel/silica (Ni/SiOx) catalyst we have conducted a series of growth experiments with a chemical vapour deposition (...
Main Authors: | Junfeng eGeng, Marcelo eMotta, Volker eAngels, Jikui eLuo, Brian F. G. Johnson |
---|---|
Format: | Article |
Language: | English |
Published: |
Frontiers Media S.A.
2016-02-01
|
Series: | Frontiers in Materials |
Subjects: | |
Online Access: | http://journal.frontiersin.org/Journal/10.3389/fmats.2016.00004/full |
Similar Items
-
Synthesis of multi-walled carbon nanotubes by thermal CVD technique on Pt–W–MgO catalyst
by: Khurshed A. Shah, et al.
Published: (2018-03-01) -
High-performance single-walled carbon nanotube transparent conducting film fabricated by using low feeding rate of ethanol solution
by: Er-Xiong Ding, et al.
Published: (2018-01-01) -
En route to controlled catalytic CVD synthesis of densely packed and vertically aligned nitrogen-doped carbon nanotube arrays
by: Slawomir Boncel, et al.
Published: (2014-03-01) -
Catalytic CVD Synthesis of Carbon Nanotubes: Towards High Yield and Low Temperature Growth
by: Marijana Mionić, et al.
Published: (2010-11-01) -
Chemical Vapour Deposition Growth of Carbon Nanotube Forests: Kinetics, Morphology, Composition, and Their Mechanisms
by: Vinten, Phillip A.
Published: (2013)