Investigation of improving wear performance of hypereutectic 15%Cr-2%Mo white irons
This study aimed at optimizing impact toughness and abrasion wear resistance of 15%Cr-2%Mo hypereutectic abrasion-resistant white irons. The effects of dynamic solidification, niobium addition, combined action of them and heat treatment have been investigated. Investigations were performed by means...
Main Authors: | R. Reda, A. Nofal, Kh. Ibrahim |
---|---|
Format: | Article |
Language: | English |
Published: |
Foundry Journal Agency
2010-11-01
|
Series: | China Foundry |
Subjects: | |
Online Access: | http://www.foundryworld.com/uploadfile/201012953225653.pdf |
Similar Items
-
Influence of Laser Welding Speed on the Morphology and Phases Occurring in Spray-Compacted Hypereutectic Al-Si-Alloys
by: Thomas Gietzelt, et al.
Published: (2016-11-01) -
Controlling Segregation Behavior of Primary Si in Hypereutectic Al-Si Alloy by Electromagnetic Stirring
by: Qingchuan Zou, et al.
Published: (2020-08-01) -
Modeling and Simulation of the Gray-to-White Transition during Solidification of a Hypereutectic Gray Cast Iron: Application to a Stub-to-Carbon Connection Used in Smelting Processes
by: Alejandro Urrutia, et al.
Published: (2017-12-01) -
Friction and wear behaviour of hypereutectic Al-Si alloy/steel tribopair under dry and lubricated conditions
by: Parveen Kumar, et al.
Published: (2017-12-01) -
In Vitro Bioactivity and Cell Biocompatibility of a Hypereutectic Bioceramic
by: Patricia Mazón, et al.
Published: (2019-03-01)