Fiber Reinforced Cement Mortars Degradation after their Exposure to Fire Conditions
Cement based mortars reinforced by glass and polypropylene fibres were exposed to fire conditions up to 900 °C from 10 min to 2 hours and after their slow cooling, were tested under compression and bending loadings. We can see that three distinct stages are appeared. At first, up to 300°C, a not...