Pengaruh beban kompaksi dan suhu sintering terhadap densitas dan sifat mekanik aluminium water atomized

The powder size used in the research were maximum of 297mm and maximum of 105m resulted by water atomization. Both powder sizes were dry mixed by ratio of 65:35 %wt and was added by 1,25% wt of wax. Mixing was taking a place in steel cylinder with diameter of 2” roteted at 140 rpm for 2 hr. Green bo...