Results of the freeze resistance test, swelling index and coefficient of permeability of finegrained mining waste reinforced with cements
The article presents the result of laboratory tests for mining waste with grain size of 0 to 2 mm stabilized with cement. Used for stabilization of cement CEM I 42.5 R and blast furnace cement CEM III / A 42.5N - LH / HSR / NA and a plasticizer sealant. Cement was added to the mining waste test in t...
Main Author: | Morman Justyna |
---|---|
Format: | Article |
Language: | English |
Published: |
EDP Sciences
2018-01-01
|
Series: | E3S Web of Conferences |
Subjects: | |
Online Access: | https://doi.org/10.1051/e3sconf/20183603004 |
Similar Items
-
Comparison of physical and mechanical properties of mining waste with a grain size up to 2 mm reinforced with cement CEM I and CEM III
by: Morman-Wątor Justyna
Published: (2019-01-01) -
Underground Cemented Backfill, a Design Procedure for an Integrated Mining Waste Management.
by: Abdelhadi KHALDOUN, et al.
Published: (2018-01-01) -
Underground Cemented Backfill, a Design Procedure for an Integrated Mining Waste Management.
by: Abdelhadi KHALDOUN, et al.
Published: (2018-01-01) -
Durability of concrete using marble mining waste
by: Sudarshan Dattatraya Kore, et al.
Published: (2016-11-01) -
Valorization and recycling of quarries waste as an addition in cement
by: Berdoudi Said, et al.
Published: (2017-01-01)