Results of the freeze resistance test, swelling index and coefficient of permeability of finegrained mining waste reinforced with cements
The article presents the result of laboratory tests for mining waste with grain size of 0 to 2 mm stabilized with cement. Used for stabilization of cement CEM I 42.5 R and blast furnace cement CEM III / A 42.5N - LH / HSR / NA and a plasticizer sealant. Cement was added to the mining waste test in t...
Main Author: | |
---|---|
Format: | Article |
Language: | English |
Published: |
EDP Sciences
2018-01-01
|
Series: | E3S Web of Conferences |
Subjects: | |
Online Access: | https://doi.org/10.1051/e3sconf/20183603004 |
Summary: | The article presents the result of laboratory tests for mining waste with grain size of 0 to 2 mm stabilized with cement. Used for stabilization of cement CEM I 42.5 R and blast furnace cement CEM III / A 42.5N - LH / HSR / NA and a plasticizer sealant. Cement was added to the mining waste test in the proportions of 5 - 8% in relation to the skeleton's weight. For the cemented samples, the freeze resistance test, swelling index, coefficient of permeability and pH of water leachate were tested. The addition of a cement binder resulted in diminishing the water permeability of mining waste and limiting the leaching of fine particles from the material. |
---|---|
ISSN: | 2267-1242 |