Low temperature spark plasma sintering of TC4/HA composites
Ti6Al4V/hydroxyapatite composites (TC4/HA) have been prepared by high energy ball milling and low temperature spark plasma sintering at 600 °C, 550 °C, 500 °C and 450 °C, respectively. The sintering temperature of the composites was sharply decreased as the result of the activation and surficial mod...
Main Authors: | Huiliang Shao, Lei Cao, Daqian Sun, Zhankui Zhao |
---|---|
Format: | Article |
Language: | English |
Published: |
Elsevier
2016-04-01
|
Series: | Progress in Natural Science: Materials International |
Subjects: | |
Online Access: | http://www.sciencedirect.com/science/article/pii/S1002007116300144 |
Similar Items
-
Fabrication of the Zirconium Diboride-Reinforced Composites by a Combination of Planetary Ball Milling, Turbula Mixing and Spark Plasma Sintering
by: Iwona Sulima, et al.
Published: (2021-07-01) -
Effects of Powder Preparation and Sintering Temperature on Properties of Spark Plasma Sintered Ti-48Al-2Cr-8Nb Alloy
by: Zhenhua Wang, et al.
Published: (2019-08-01) -
Compressive strength and thermal properties of spark plasma sintered Al-Al2O3 nanocomposite
by: Saheb Nouari, et al.
Published: (2018-01-01) -
Reactive Spark Plasma Sintering and Mechanical Properties of Zirconium Diboride–Titanium Diboride Ultrahigh Temperature Ceramic Solid Solutions
by: Karthiselva N. S., et al.
Published: (2016-09-01) -
Colossal relative permittivity and low dielectric loss in BaFe0.5Nb0.5O3 ceramics prepared by spark plasma sintering
by: H. Mahfoz Kotb, et al.
Published: (2020-12-01)