Preparation of Ta/W Composite by CVD
The Ta/W composites with 10%W, 13%W and 18%W were prepared by chemical vapor deposition (CVD). The properties of Ta/W composites were investigated by optical microscopy (OM), scanning electron microscopy (SEM ) and tensile test. The results show that it is possible to prepare Ta/W composites with di...
Main Authors: | , , , , , |
---|---|
Format: | Article |
Language: | zho |
Published: |
Journal of Aeronautical Materials
2017-04-01
|
Series: | Journal of Aeronautical Materials |
Subjects: | |
Online Access: | http://jam.biam.ac.cn/CN/Y2017/V37/I2/38 |
id |
doaj-731751dea2df4276a59440e407e5d143 |
---|---|
record_format |
Article |
spelling |
doaj-731751dea2df4276a59440e407e5d1432020-11-24T21:50:58ZzhoJournal of Aeronautical MaterialsJournal of Aeronautical Materials1005-50531005-50532017-04-01372384310.11868/j.issn.1005-5053.2016.000019201702000019Preparation of Ta/W Composite by CVDQI Xiaohong0ZHENG Xu1CAI Hongzhong2LIU Shaopeng3HU Changyi4WEI Yan5State Key Laboratory of Advanced Technologies for Comprehensive Utilization of Platinum Metals, Kunming Institute of Precious Metals, Kunming 650106, ChinaState Key Laboratory of Advanced Technologies for Comprehensive Utilization of Platinum Metals, Kunming Institute of Precious Metals, Kunming 650106, ChinaState Key Laboratory of Advanced Technologies for Comprehensive Utilization of Platinum Metals, Kunming Institute of Precious Metals, Kunming 650106, ChinaState Key Laboratory of Advanced Technologies for Comprehensive Utilization of Platinum Metals, Kunming Institute of Precious Metals, Kunming 650106, ChinaState Key Laboratory of Advanced Technologies for Comprehensive Utilization of Platinum Metals, Kunming Institute of Precious Metals, Kunming 650106, ChinaState Key Laboratory of Advanced Technologies for Comprehensive Utilization of Platinum Metals, Kunming Institute of Precious Metals, Kunming 650106, ChinaThe Ta/W composites with 10%W, 13%W and 18%W were prepared by chemical vapor deposition (CVD). The properties of Ta/W composites were investigated by optical microscopy (OM), scanning electron microscopy (SEM ) and tensile test. The results show that it is possible to prepare Ta/W composites with different W volume fractions by CVD, and the actual densities of the composites are more than 99.4% of the theoretical density. Both Ta and W layers have columnar grain structures, and the more close to the interface, the more fine the grains are. The mechanical properties of CVD Ta/W are better than those of CVD Ta or CVD W. After hot treatment(1600 ℃×2 h),the diffused layers of the composites have become more wider and the mechanical properties are increased remarkably, and the tensile strength of the CVD Ta/W composite with 18%W is 660 MPa.http://jam.biam.ac.cn/CN/Y2017/V37/I2/38chemical vapor deposition (CVD)Ta/W compositevolume fraction of Wmechanical properties |
collection |
DOAJ |
language |
zho |
format |
Article |
sources |
DOAJ |
author |
QI Xiaohong ZHENG Xu CAI Hongzhong LIU Shaopeng HU Changyi WEI Yan |
spellingShingle |
QI Xiaohong ZHENG Xu CAI Hongzhong LIU Shaopeng HU Changyi WEI Yan Preparation of Ta/W Composite by CVD Journal of Aeronautical Materials chemical vapor deposition (CVD) Ta/W composite volume fraction of W mechanical properties |
author_facet |
QI Xiaohong ZHENG Xu CAI Hongzhong LIU Shaopeng HU Changyi WEI Yan |
author_sort |
QI Xiaohong |
title |
Preparation of Ta/W Composite by CVD |
title_short |
Preparation of Ta/W Composite by CVD |
title_full |
Preparation of Ta/W Composite by CVD |
title_fullStr |
Preparation of Ta/W Composite by CVD |
title_full_unstemmed |
Preparation of Ta/W Composite by CVD |
title_sort |
preparation of ta/w composite by cvd |
publisher |
Journal of Aeronautical Materials |
series |
Journal of Aeronautical Materials |
issn |
1005-5053 1005-5053 |
publishDate |
2017-04-01 |
description |
The Ta/W composites with 10%W, 13%W and 18%W were prepared by chemical vapor deposition (CVD). The properties of Ta/W composites were investigated by optical microscopy (OM), scanning electron microscopy (SEM ) and tensile test. The results show that it is possible to prepare Ta/W composites with different W volume fractions by CVD, and the actual densities of the composites are more than 99.4% of the theoretical density. Both Ta and W layers have columnar grain structures, and the more close to the interface, the more fine the grains are. The mechanical properties of CVD Ta/W are better than those of CVD Ta or CVD W. After hot treatment(1600 ℃×2 h),the diffused layers of the composites have become more wider and the mechanical properties are increased remarkably, and the tensile strength of the CVD Ta/W composite with 18%W is 660 MPa. |
topic |
chemical vapor deposition (CVD) Ta/W composite volume fraction of W mechanical properties |
url |
http://jam.biam.ac.cn/CN/Y2017/V37/I2/38 |
work_keys_str_mv |
AT qixiaohong preparationoftawcompositebycvd AT zhengxu preparationoftawcompositebycvd AT caihongzhong preparationoftawcompositebycvd AT liushaopeng preparationoftawcompositebycvd AT huchangyi preparationoftawcompositebycvd AT weiyan preparationoftawcompositebycvd |
_version_ |
1725881329998888960 |