Effect of the change of firing temperature on microstructure and physical properties of clay bricks from Beruas (Malaysia)

This study is focused on the behaviour of fired-clay brick from the area around Beruas (Malaysia) that is known for it brick industries. The firing temperatures were set from 800°C to 1250°C and soaking time was fixed for an hour. The effects of firing temperature on the phase changes, microstruc...