Recycling Y and Eu from Waste Fluorescent Powder and High Temperature Solid-State Synthesis of Y2O3:Eu Phosphors
Y2O3:Eu were prepared through precursors synthesized by leaching tests, removing impurities, enrichment of Y and Eu from residual purified liquors, annealing treatment, and high temperature solid-state reaction method, which is the most suitable for large-scale production. The analysis of product sh...
Main Authors: | Xiaodong Chen, Nian Liu, Guangjun Mei, Mingming Yu |
---|---|
Format: | Article |
Language: | English |
Published: |
MDPI AG
2017-03-01
|
Series: | Minerals |
Subjects: | |
Online Access: | http://www.mdpi.com/2075-163X/7/3/44 |
Similar Items
-
Recovering Y and Eu from Waste Phosphors Using Chlorination Roasting—Water Leaching Process
by: Mingming Yu, et al.
Published: (2016-10-01) -
Solvent Extraction of Ni and Co from the Phosphoric Acid Leaching Solution of Laterite Ore by P204 and P507
by: Mingjun Rao, et al.
Published: (2020-04-01) -
Impurity removal process for high-purity silica production by acid leaching
by: Ezzaouia H., et al.
Published: (2012-06-01) -
First impurity powder injection experiments in LHD
by: F. Nespoli, et al.
Published: (2020-12-01) -
Hydrothermal synthesis and luminescent properties of Y2O3:Eu3+ from waste phosphors
by: Mingming Yu, et al.
Published: (2018-09-01)