Enhanced piezoelectric properties of (Ba0.3Bi0.7)(Mg0.05Fe0.6Ti0.35)O3 piezoelectric ceramics with high Curie temperature
(Ba0.3Bi0.7)(Mg0.05Fe0.6Ti0.35)O3 ceramics were either doped with vanadium or sintered in calcined powder with the same composition. Compared to an undoped ceramic sintered without the calcined powder, both ceramics showed reduced leakage current densities (lower than 1 × 10-7 A/cm2) and absence of...