Preparation of Anodic Aluminum Oxide Masks with Size-Controlled Pores for 2D Plasmonic Nanodot Arrays

Anodic aluminum oxide (AAO) layers with nano-sized pores have been used as shadow masks for the fabrication of two-dimensional (2D) metal nanodot arrays (NDAs). However, the localized surface plasmon resonance (LSPR) of size-controlled NDAs fabricated using AAO masks has not been much studied. In th...

Full description

Bibliographic Details
Main Authors: Mi Jung, Ji-Hoon Kim, Young-Wan Choi
Format: Article
Language:English
Published: Hindawi Limited 2018-01-01
Series:Journal of Nanomaterials
Online Access:http://dx.doi.org/10.1155/2018/6249890
id doaj-56fc79c33dce4ad996bc0e25b70ac677
record_format Article
spelling doaj-56fc79c33dce4ad996bc0e25b70ac6772020-11-24T20:56:05ZengHindawi LimitedJournal of Nanomaterials1687-41101687-41292018-01-01201810.1155/2018/62498906249890Preparation of Anodic Aluminum Oxide Masks with Size-Controlled Pores for 2D Plasmonic Nanodot ArraysMi Jung0Ji-Hoon Kim1Young-Wan Choi2Institute of Innovative Functional Imaging, Chung-Ang University, Seoul 06974, Republic of KoreaSchool of Electrical and Electronics Engineering, Chung-Ang University, Seoul 06974, Republic of KoreaSchool of Electrical and Electronics Engineering, Chung-Ang University, Seoul 06974, Republic of KoreaAnodic aluminum oxide (AAO) layers with nano-sized pores have been used as shadow masks for the fabrication of two-dimensional (2D) metal nanodot arrays (NDAs). However, the localized surface plasmon resonance (LSPR) of size-controlled NDAs fabricated using AAO masks has not been much studied. In this study, we report on the improved preparation method and utilization of an ultrathin AAO mask for the fabrication of 2D plasmonic metal NDAs. The greatest challenge in preparing an AAO mask is to control the pore diameter and to make it reproducible. AAO masks with size-controlled pores were reproducibly prepared using a two-step chemical wet etching method. Ag NDAs with different dot diameters (42, 60, and 80 nm) and Ag, Cu, and Au NDAs with dot a diameter of 80 ± 5 nm were fabricated on indium tin oxide glass substrates using AAO masks. The wavelengths corresponding to LSPR of 2D metal NDAs were investigated using ultraviolet–visible spectroscopy. Our results show that AAO masks with tunable pores can be used as shadow masks for the fabrication of 2D plasmonic NDAs.http://dx.doi.org/10.1155/2018/6249890
collection DOAJ
language English
format Article
sources DOAJ
author Mi Jung
Ji-Hoon Kim
Young-Wan Choi
spellingShingle Mi Jung
Ji-Hoon Kim
Young-Wan Choi
Preparation of Anodic Aluminum Oxide Masks with Size-Controlled Pores for 2D Plasmonic Nanodot Arrays
Journal of Nanomaterials
author_facet Mi Jung
Ji-Hoon Kim
Young-Wan Choi
author_sort Mi Jung
title Preparation of Anodic Aluminum Oxide Masks with Size-Controlled Pores for 2D Plasmonic Nanodot Arrays
title_short Preparation of Anodic Aluminum Oxide Masks with Size-Controlled Pores for 2D Plasmonic Nanodot Arrays
title_full Preparation of Anodic Aluminum Oxide Masks with Size-Controlled Pores for 2D Plasmonic Nanodot Arrays
title_fullStr Preparation of Anodic Aluminum Oxide Masks with Size-Controlled Pores for 2D Plasmonic Nanodot Arrays
title_full_unstemmed Preparation of Anodic Aluminum Oxide Masks with Size-Controlled Pores for 2D Plasmonic Nanodot Arrays
title_sort preparation of anodic aluminum oxide masks with size-controlled pores for 2d plasmonic nanodot arrays
publisher Hindawi Limited
series Journal of Nanomaterials
issn 1687-4110
1687-4129
publishDate 2018-01-01
description Anodic aluminum oxide (AAO) layers with nano-sized pores have been used as shadow masks for the fabrication of two-dimensional (2D) metal nanodot arrays (NDAs). However, the localized surface plasmon resonance (LSPR) of size-controlled NDAs fabricated using AAO masks has not been much studied. In this study, we report on the improved preparation method and utilization of an ultrathin AAO mask for the fabrication of 2D plasmonic metal NDAs. The greatest challenge in preparing an AAO mask is to control the pore diameter and to make it reproducible. AAO masks with size-controlled pores were reproducibly prepared using a two-step chemical wet etching method. Ag NDAs with different dot diameters (42, 60, and 80 nm) and Ag, Cu, and Au NDAs with dot a diameter of 80 ± 5 nm were fabricated on indium tin oxide glass substrates using AAO masks. The wavelengths corresponding to LSPR of 2D metal NDAs were investigated using ultraviolet–visible spectroscopy. Our results show that AAO masks with tunable pores can be used as shadow masks for the fabrication of 2D plasmonic NDAs.
url http://dx.doi.org/10.1155/2018/6249890
work_keys_str_mv AT mijung preparationofanodicaluminumoxidemaskswithsizecontrolledporesfor2dplasmonicnanodotarrays
AT jihoonkim preparationofanodicaluminumoxidemaskswithsizecontrolledporesfor2dplasmonicnanodotarrays
AT youngwanchoi preparationofanodicaluminumoxidemaskswithsizecontrolledporesfor2dplasmonicnanodotarrays
_version_ 1716790789596512256