Effect of solidification parameters on the microstructures of a single crystal Ni-based superalloy AM3
A single crystal Ni-based superalloy AM3 was processed at withdraw rates of 3.5, 10, 50, 100, 200, and 500 μm•s-1, respectively. The as-cast microstructures and solidification segregation ratio were characterized with various withdraw rates. The shape and size of carbide microstructures were determi...
Main Authors: | Yu Zhuhuan, Liu Lin, Zhao Xinbao |
---|---|
Format: | Article |
Language: | English |
Published: |
Foundry Journal Agency
2010-08-01
|
Series: | China Foundry |
Subjects: | |
Online Access: | http://www.foundryworld.com/uploadfile/2010112351333565.pdf |
Similar Items
-
Effect of carbon additions on the microstructure of a single crystal Ni-based superalloy AM3
by: Yu Zhuhuan, et al.
Published: (2010-11-01) -
Sliver defect formation in single crystal Ni-based superalloy castings
by: Wenliang Xu, et al.
Published: (2020-11-01) -
Processing, Microstructures and Mechanical Properties of a Ni-Based Single Crystal Superalloy
by: Qingqing Ding, et al.
Published: (2020-07-01) -
Grain Selection in a High-Efficiency 2D Grain Selector During Casting of Single-Crystal Superalloys
by: Xintao Zhu, et al.
Published: (2019-03-01) -
Effect of Solidification Behavior on Microstructures and Mechanical Properties of Ni-Cr-Fe Superalloy Investment Casting
by: Maodong Kang, et al.
Published: (2017-03-01)