Characterization of recycled crumb rubber modified binders containing wax warm additives
This paper addresses the laboratory experiment of performance properties of recycled CRM binders containing artificially aged CRM binders with wax additives. The warm CRM binders were produced using two wax additives (LEADCAP and Sasobit) and then short-term and long-term aged using the rolling thin...
Main Authors: | , , , |
---|---|
Format: | Article |
Language: | English |
Published: |
KeAi Communications Co., Ltd.
2018-06-01
|
Series: | Journal of Traffic and Transportation Engineering (English ed. Online) |
Online Access: | http://www.sciencedirect.com/science/article/pii/S2095756417302660 |
id |
doaj-3c097e0f847b469a8e5eec495d8605aa |
---|---|
record_format |
Article |
spelling |
doaj-3c097e0f847b469a8e5eec495d8605aa2021-02-02T02:17:34ZengKeAi Communications Co., Ltd.Journal of Traffic and Transportation Engineering (English ed. Online)2095-75642018-06-0153197206Characterization of recycled crumb rubber modified binders containing wax warm additivesHyun Hwan Kim0Mithil Mazumder1Soon-Jae Lee2Moon-Sup Lee3Department of Engineering Technology, Texas State University, San Marcos, TX 78666, USAMaterials Science, Engineering, and Commercialization Program, Texas State University, San Marcos, TX 78666, USADepartment of Engineering Technology, Texas State University, San Marcos, TX 78666, USAKorea Institute of Civil Engineering and Building Technology, Goyang-si, Gyeonggi-do 10223, Republic of Korea; Corresponding author. Tel.: +1 512 245 2137; fax: +1 512 245 3052.This paper addresses the laboratory experiment of performance properties of recycled CRM binders containing artificially aged CRM binders with wax additives. The warm CRM binders were produced using two wax additives (LEADCAP and Sasobit) and then short-term and long-term aged using the rolling thin film oven (RTFO) and pressure aging vessel (PAV) procedures. The recycled CRM binders were aged through the RTFO and PAV procedures. A set of Superpave binder tests were carried out on the binders through the rotational viscometer, the dynamic shear rheometer (DSR), and the bending beam rheometer (BBR). In general, the results of this study indicated that (1) the addition of long-term aged (LTA) CRM binder can significantly increase the viscosity of the recycled CRM binders as expected, (2) the wax additives in recycled CRM binders were still effective to improve the viscosity and rutting properties even after experiencing the aging process, (3) the CRM binders containing wax additives showed the higher rutting resistance compared to the control CRM binders, (4) the recycled CRM binder containing wax additives was found to have less resistance to fatigue and low temperature cracking, (5) wax warm additives into the recycled CRM binders seemed to have a significant role for cracking properties, based upon their substantial amount. Keywords: CRM binder, Wax additives, Rotational viscosity, Recycling, Ruttinghttp://www.sciencedirect.com/science/article/pii/S2095756417302660 |
collection |
DOAJ |
language |
English |
format |
Article |
sources |
DOAJ |
author |
Hyun Hwan Kim Mithil Mazumder Soon-Jae Lee Moon-Sup Lee |
spellingShingle |
Hyun Hwan Kim Mithil Mazumder Soon-Jae Lee Moon-Sup Lee Characterization of recycled crumb rubber modified binders containing wax warm additives Journal of Traffic and Transportation Engineering (English ed. Online) |
author_facet |
Hyun Hwan Kim Mithil Mazumder Soon-Jae Lee Moon-Sup Lee |
author_sort |
Hyun Hwan Kim |
title |
Characterization of recycled crumb rubber modified binders containing wax warm additives |
title_short |
Characterization of recycled crumb rubber modified binders containing wax warm additives |
title_full |
Characterization of recycled crumb rubber modified binders containing wax warm additives |
title_fullStr |
Characterization of recycled crumb rubber modified binders containing wax warm additives |
title_full_unstemmed |
Characterization of recycled crumb rubber modified binders containing wax warm additives |
title_sort |
characterization of recycled crumb rubber modified binders containing wax warm additives |
publisher |
KeAi Communications Co., Ltd. |
series |
Journal of Traffic and Transportation Engineering (English ed. Online) |
issn |
2095-7564 |
publishDate |
2018-06-01 |
description |
This paper addresses the laboratory experiment of performance properties of recycled CRM binders containing artificially aged CRM binders with wax additives. The warm CRM binders were produced using two wax additives (LEADCAP and Sasobit) and then short-term and long-term aged using the rolling thin film oven (RTFO) and pressure aging vessel (PAV) procedures. The recycled CRM binders were aged through the RTFO and PAV procedures. A set of Superpave binder tests were carried out on the binders through the rotational viscometer, the dynamic shear rheometer (DSR), and the bending beam rheometer (BBR). In general, the results of this study indicated that (1) the addition of long-term aged (LTA) CRM binder can significantly increase the viscosity of the recycled CRM binders as expected, (2) the wax additives in recycled CRM binders were still effective to improve the viscosity and rutting properties even after experiencing the aging process, (3) the CRM binders containing wax additives showed the higher rutting resistance compared to the control CRM binders, (4) the recycled CRM binder containing wax additives was found to have less resistance to fatigue and low temperature cracking, (5) wax warm additives into the recycled CRM binders seemed to have a significant role for cracking properties, based upon their substantial amount. Keywords: CRM binder, Wax additives, Rotational viscosity, Recycling, Rutting |
url |
http://www.sciencedirect.com/science/article/pii/S2095756417302660 |
work_keys_str_mv |
AT hyunhwankim characterizationofrecycledcrumbrubbermodifiedbinderscontainingwaxwarmadditives AT mithilmazumder characterizationofrecycledcrumbrubbermodifiedbinderscontainingwaxwarmadditives AT soonjaelee characterizationofrecycledcrumbrubbermodifiedbinderscontainingwaxwarmadditives AT moonsuplee characterizationofrecycledcrumbrubbermodifiedbinderscontainingwaxwarmadditives |
_version_ |
1724310125662961664 |