FEATURES OF WELDED TITANIUM STRUCTURE ELEMENT DESTRUCTION (RIBBED PANELS) UNDER VIBRATION LOADS
The article presents data on the experimental studies results of welded ribbed panel vibration load of the BT-20 titanium alloy. It was established that in the areas of attachment, there is elevated dynamic alternating stress, which in combination with the "hard" of the sample holder creat...
Main Authors: | , , |
---|---|
Format: | Article |
Language: | Russian |
Published: |
Komsomolsk-na-Amure State Technical University
2016-12-01
|
Series: | Učenye Zapiski Komsomolʹskogo-na-Amure Gosudarstvennogo Tehničeskogo Universiteta |
Subjects: | |
Online Access: | http://www.uzknastu.ru/files/pdf/28/1/14.pdf |
id |
doaj-2c5da8fd7a7b4a78aff1e99dbf27984d |
---|---|
record_format |
Article |
spelling |
doaj-2c5da8fd7a7b4a78aff1e99dbf27984d2020-11-24T22:42:32ZrusKomsomolsk-na-Amure State Technical UniversityUčenye Zapiski Komsomolʹskogo-na-Amure Gosudarstvennogo Tehničeskogo Universiteta2076-43592222-52182016-12-011110410910.17084/2016.IV-1(28).142016-28-1-14FEATURES OF WELDED TITANIUM STRUCTURE ELEMENT DESTRUCTION (RIBBED PANELS) UNDER VIBRATION LOADSMr. Pavel V. Bakhmatov0Mr. Vasiliy I. Muravyev1Mr. Roman A. Fizulakov2Komsomolsk-on-Amur state technical universityKomsomolsk-on-Amur state technical universityKomsomolsk-on-Amur state technical universityThe article presents data on the experimental studies results of welded ribbed panel vibration load of the BT-20 titanium alloy. It was established that in the areas of attachment, there is elevated dynamic alternating stress, which in combination with the "hard" of the sample holder creates favorable conditions for the emergence and development of fatigue cracks, and stress concentrators greatly reduce the time before the formation of the hearth destruction. An exception in these zones of superficial defects do not affect the nature and kinetics of destruction. Construction of titanium alloys made in the application of gas-laser cutting blanks for optimal regimes in the technical environment of nitrogen and subsequent heat treatment on vibration reliability is not inferior to design, made by traditional technology.http://www.uzknastu.ru/files/pdf/28/1/14.pdfcyclic strengthdynamic loadstitanium ribbed welded structureswelding modesdestruction |
collection |
DOAJ |
language |
Russian |
format |
Article |
sources |
DOAJ |
author |
Mr. Pavel V. Bakhmatov Mr. Vasiliy I. Muravyev Mr. Roman A. Fizulakov |
spellingShingle |
Mr. Pavel V. Bakhmatov Mr. Vasiliy I. Muravyev Mr. Roman A. Fizulakov FEATURES OF WELDED TITANIUM STRUCTURE ELEMENT DESTRUCTION (RIBBED PANELS) UNDER VIBRATION LOADS Učenye Zapiski Komsomolʹskogo-na-Amure Gosudarstvennogo Tehničeskogo Universiteta cyclic strength dynamic loads titanium ribbed welded structures welding modes destruction |
author_facet |
Mr. Pavel V. Bakhmatov Mr. Vasiliy I. Muravyev Mr. Roman A. Fizulakov |
author_sort |
Mr. Pavel V. Bakhmatov |
title |
FEATURES OF WELDED TITANIUM STRUCTURE ELEMENT DESTRUCTION (RIBBED PANELS) UNDER VIBRATION LOADS |
title_short |
FEATURES OF WELDED TITANIUM STRUCTURE ELEMENT DESTRUCTION (RIBBED PANELS) UNDER VIBRATION LOADS |
title_full |
FEATURES OF WELDED TITANIUM STRUCTURE ELEMENT DESTRUCTION (RIBBED PANELS) UNDER VIBRATION LOADS |
title_fullStr |
FEATURES OF WELDED TITANIUM STRUCTURE ELEMENT DESTRUCTION (RIBBED PANELS) UNDER VIBRATION LOADS |
title_full_unstemmed |
FEATURES OF WELDED TITANIUM STRUCTURE ELEMENT DESTRUCTION (RIBBED PANELS) UNDER VIBRATION LOADS |
title_sort |
features of welded titanium structure element destruction (ribbed panels) under vibration loads |
publisher |
Komsomolsk-na-Amure State Technical University |
series |
Učenye Zapiski Komsomolʹskogo-na-Amure Gosudarstvennogo Tehničeskogo Universiteta |
issn |
2076-4359 2222-5218 |
publishDate |
2016-12-01 |
description |
The article presents data on the experimental studies results of welded ribbed panel vibration load of the BT-20 titanium alloy. It was established that in the areas of attachment, there is elevated dynamic alternating stress, which in combination with the "hard" of the sample holder creates favorable conditions for the emergence and development of fatigue cracks, and stress concentrators greatly reduce the time before the formation of the hearth destruction. An exception in these zones of superficial defects do not affect the nature and kinetics of destruction. Construction of titanium alloys made in the application of gas-laser cutting blanks for optimal regimes in the technical environment of nitrogen and subsequent heat treatment on vibration reliability is not inferior to design, made by traditional technology. |
topic |
cyclic strength dynamic loads titanium ribbed welded structures welding modes destruction |
url |
http://www.uzknastu.ru/files/pdf/28/1/14.pdf |
work_keys_str_mv |
AT mrpavelvbakhmatov featuresofweldedtitaniumstructureelementdestructionribbedpanelsundervibrationloads AT mrvasiliyimuravyev featuresofweldedtitaniumstructureelementdestructionribbedpanelsundervibrationloads AT mrromanafizulakov featuresofweldedtitaniumstructureelementdestructionribbedpanelsundervibrationloads |
_version_ |
1725699512636276736 |