Durability of oil-based caulking compound and rubber gaskets applied in panel joints of the old living hut built in 1969 at Syowa Station, Antarctica
Deterioration of aged oil-based caulking and rubber gaskets that had been used for sealing in the joints between wall panels of the old living hut built in 1969 at Syowa Station was studied. As for oil-based caulking, tack and penetration measurements were carried out. The caulking turned from flexi...
Main Authors: | , , |
---|---|
Format: | Article |
Language: | English |
Published: |
National Institute of Polar Research
2002-09-01
|
Series: | Antarctic Record |
Online Access: | http://doi.org/10.15094/00009246 |
id |
doaj-29bf6a1bd0a6432cb7066be694a3cb17 |
---|---|
record_format |
Article |
spelling |
doaj-29bf6a1bd0a6432cb7066be694a3cb172020-11-24T23:41:41ZengNational Institute of Polar ResearchAntarctic Record0085-72892432-079X2002-09-01462A51852410.15094/00009246Durability of oil-based caulking compound and rubber gaskets applied in panel joints of the old living hut built in 1969 at Syowa Station, Antarctica Kyoji Tanaka0Ichirou Shimizu1Yuko Suda2Structual Engineering Research Center, Tokyo Institute of Technologyapan Testing Center For Construction MaterialsGraduate school, Tokyo Institute of TechnologyDeterioration of aged oil-based caulking and rubber gaskets that had been used for sealing in the joints between wall panels of the old living hut built in 1969 at Syowa Station was studied. As for oil-based caulking, tack and penetration measurements were carried out. The caulking turned from flexible to brittle in mechanical property by degradation. Fortunately, no water leakage from the joints was reported in the service period of the building though the material had not severely moved by rigid structural design. As for rubber gaskets, appearance observation, tensile and hardness tests were carried out, they keep at good level in mechanical property, however severe cracks occurred on their surfaces, and they were judged to have reached the limit of their useful lifetimes. http://doi.org/10.15094/00009246 |
collection |
DOAJ |
language |
English |
format |
Article |
sources |
DOAJ |
author |
Kyoji Tanaka Ichirou Shimizu Yuko Suda |
spellingShingle |
Kyoji Tanaka Ichirou Shimizu Yuko Suda Durability of oil-based caulking compound and rubber gaskets applied in panel joints of the old living hut built in 1969 at Syowa Station, Antarctica Antarctic Record |
author_facet |
Kyoji Tanaka Ichirou Shimizu Yuko Suda |
author_sort |
Kyoji Tanaka |
title |
Durability of oil-based caulking compound and rubber gaskets applied in panel joints of the old living hut built in 1969 at Syowa Station, Antarctica |
title_short |
Durability of oil-based caulking compound and rubber gaskets applied in panel joints of the old living hut built in 1969 at Syowa Station, Antarctica |
title_full |
Durability of oil-based caulking compound and rubber gaskets applied in panel joints of the old living hut built in 1969 at Syowa Station, Antarctica |
title_fullStr |
Durability of oil-based caulking compound and rubber gaskets applied in panel joints of the old living hut built in 1969 at Syowa Station, Antarctica |
title_full_unstemmed |
Durability of oil-based caulking compound and rubber gaskets applied in panel joints of the old living hut built in 1969 at Syowa Station, Antarctica |
title_sort |
durability of oil-based caulking compound and rubber gaskets applied in panel joints of the old living hut built in 1969 at syowa station, antarctica |
publisher |
National Institute of Polar Research |
series |
Antarctic Record |
issn |
0085-7289 2432-079X |
publishDate |
2002-09-01 |
description |
Deterioration of aged oil-based caulking and rubber gaskets that had been used for sealing in the joints between wall panels of the old living hut built in 1969 at Syowa Station was studied. As for oil-based caulking, tack and penetration measurements were carried out. The caulking turned from flexible to brittle in mechanical property by degradation. Fortunately, no water leakage from the joints was reported in the service period of the building though the material had not severely moved by rigid structural design. As for rubber gaskets, appearance observation, tensile and hardness tests were carried out, they keep at good level in mechanical property, however severe cracks occurred on their surfaces, and they were judged to have reached the limit of their useful lifetimes. |
url |
http://doi.org/10.15094/00009246 |
work_keys_str_mv |
AT kyojitanaka durabilityofoilbasedcaulkingcompoundandrubbergasketsappliedinpaneljointsoftheoldlivinghutbuiltin1969atsyowastationantarctica AT ichiroushimizu durabilityofoilbasedcaulkingcompoundandrubbergasketsappliedinpaneljointsoftheoldlivinghutbuiltin1969atsyowastationantarctica AT yukosuda durabilityofoilbasedcaulkingcompoundandrubbergasketsappliedinpaneljointsoftheoldlivinghutbuiltin1969atsyowastationantarctica |
_version_ |
1725505937066688512 |