Lowering ash slagging and fouling tendency of high-alkali coal by hydrothermal pretreatment
High-alkali species in coal are notorious for causing ash slagging and fouling incidents. In this paper, four high-alkali coals were individually subject to hydrothermal pretreatment (HTP), within a batch-type autoclave at 300 °C for 1 h, and the treated coals were analyzed, along with the oxygen-co...
Main Authors: | Mingshun Yang, Qiang Xie, Xin Wang, He Dong, Hao Zhang, Chunqi Li |
---|---|
Format: | Article |
Language: | English |
Published: |
Elsevier
2019-05-01
|
Series: | International Journal of Mining Science and Technology |
Online Access: | http://www.sciencedirect.com/science/article/pii/S209526861730678X |
Similar Items
-
Alkali-activated Slag Binders with BOF Slag and Fly Ash
by: Chung-HoTsai, et al.
Published: (2011) -
The formation of fouling and slagging deposits in pulverized coal combustion
by: Loehden, David Otto
Published: (2005) -
The Influence of Ashing Temperature on Ash Fouling and Slagging Characteristics during Combustion of Biomass Fuels
by: Xiwen Yao, et al.
Published: (2017-01-01) -
Properties of alkali-activated slag-fly ash concrete
by: Wei,Rui-Jun, et al.
Published: (2018) -
Effects of Fly Ash on the properties of Alkali Activated Slag Concrete
by: Kothari, Ankit
Published: (2017)