Fractomechanical Properties of As-Cast and Austempered SG Cast Iron Between -40 °C and +20 °C
The spheroidal graphite (SG) cast iron fractomechanical response varies with the test temperature and with the microstructure parameters. In the present paper, we analyze this variation performing fractomechanical tests in a temperature range from -40°C to +20°C, doing also Charpy and tensile tests...
Main Authors: | V.E. Fierro, J.A. Sikora, F.R. Agüera, H.N. Alvarez Villar, A.F. Ansaldi, P.J.J. Ratto |
---|---|
Format: | Article |
Language: | English |
Published: |
Associação Brasileira de Metalurgia e Materiais (ABM); Associação Brasileira de Cerâmica (ABC); Associação Brasileira de Polímeros (ABPol)
2002-06-01
|
Series: | Materials Research |
Subjects: | |
Online Access: | http://www.scielo.br/scielo.php?script=sci_arttext&pid=S1516-14392002000200009 |
Similar Items
-
The abrasion of austempered cast iron in laboratory and work conditions
by: Roman Březina, et al.
Published: (2005-01-01) -
Evaluation of Volume Fraction of Austenite in Austempering Process of Austempered Ductile Iron
by: Edward Tyrała, et al.
Published: (2019-08-01) -
Effect of austempering temperature and manganese content on the impact energy of austempered ductile iron
by: Ananda Hegde, et al.
Published: (2021-01-01) -
Properties investigation of austempered ductile iron
by: Sudhanshu Detwal, et al.
Published: (2016-03-01) -
Influece of the austempering temperature on the tensile strength of the austempered ductile iron (ADI) samples
by: S. Savićević, et al.
Published: (2017-01-01)