Fractomechanical Properties of As-Cast and Austempered SG Cast Iron Between -40 °C and +20 °C
The spheroidal graphite (SG) cast iron fractomechanical response varies with the test temperature and with the microstructure parameters. In the present paper, we analyze this variation performing fractomechanical tests in a temperature range from -40°C to +20°C, doing also Charpy and tensile tests...
Main Authors: | , , , , , |
---|---|
Format: | Article |
Language: | English |
Published: |
Associação Brasileira de Metalurgia e Materiais (ABM); Associação Brasileira de Cerâmica (ABC); Associação Brasileira de Polímeros (ABPol)
2002-06-01
|
Series: | Materials Research |
Subjects: | |
Online Access: | http://www.scielo.br/scielo.php?script=sci_arttext&pid=S1516-14392002000200009 |
id |
doaj-22527c5eba844f1e8f4729d44c892950 |
---|---|
record_format |
Article |
spelling |
doaj-22527c5eba844f1e8f4729d44c8929502020-11-24T23:09:54ZengAssociação Brasileira de Metalurgia e Materiais (ABM); Associação Brasileira de Cerâmica (ABC); Associação Brasileira de Polímeros (ABPol)Materials Research1516-14392002-06-015213714110.1590/S1516-14392002000200009Fractomechanical Properties of As-Cast and Austempered SG Cast Iron Between -40 °C and +20 °CV.E. FierroJ.A. SikoraF.R. AgüeraH.N. Alvarez VillarA.F. AnsaldiP.J.J. RattoThe spheroidal graphite (SG) cast iron fractomechanical response varies with the test temperature and with the microstructure parameters. In the present paper, we analyze this variation performing fractomechanical tests in a temperature range from -40°C to +20°C, doing also Charpy and tensile tests for material characterization. The tests were carried out on as-cast samples and heat treated samples to obtain an ADI grade 1. In both cases, we studied samples taken from two well differentiated "Y" block sizes. The results obtained show that, for the chemical composition analyzed, both castings have a fractomechanical response decrease as the temperature diminishes. Besides, the block size enlargement produce a deterioration of the mechanical properties (the fracture toughness, mainly), for both castings.http://www.scielo.br/scielo.php?script=sci_arttext&pid=S1516-14392002000200009cast ironADIfractomechanicslow temperature |
collection |
DOAJ |
language |
English |
format |
Article |
sources |
DOAJ |
author |
V.E. Fierro J.A. Sikora F.R. Agüera H.N. Alvarez Villar A.F. Ansaldi P.J.J. Ratto |
spellingShingle |
V.E. Fierro J.A. Sikora F.R. Agüera H.N. Alvarez Villar A.F. Ansaldi P.J.J. Ratto Fractomechanical Properties of As-Cast and Austempered SG Cast Iron Between -40 °C and +20 °C Materials Research cast iron ADI fractomechanics low temperature |
author_facet |
V.E. Fierro J.A. Sikora F.R. Agüera H.N. Alvarez Villar A.F. Ansaldi P.J.J. Ratto |
author_sort |
V.E. Fierro |
title |
Fractomechanical Properties of As-Cast and Austempered SG Cast Iron Between -40 °C and +20 °C |
title_short |
Fractomechanical Properties of As-Cast and Austempered SG Cast Iron Between -40 °C and +20 °C |
title_full |
Fractomechanical Properties of As-Cast and Austempered SG Cast Iron Between -40 °C and +20 °C |
title_fullStr |
Fractomechanical Properties of As-Cast and Austempered SG Cast Iron Between -40 °C and +20 °C |
title_full_unstemmed |
Fractomechanical Properties of As-Cast and Austempered SG Cast Iron Between -40 °C and +20 °C |
title_sort |
fractomechanical properties of as-cast and austempered sg cast iron between -40 °c and +20 °c |
publisher |
Associação Brasileira de Metalurgia e Materiais (ABM); Associação Brasileira de Cerâmica (ABC); Associação Brasileira de Polímeros (ABPol) |
series |
Materials Research |
issn |
1516-1439 |
publishDate |
2002-06-01 |
description |
The spheroidal graphite (SG) cast iron fractomechanical response varies with the test temperature and with the microstructure parameters. In the present paper, we analyze this variation performing fractomechanical tests in a temperature range from -40°C to +20°C, doing also Charpy and tensile tests for material characterization. The tests were carried out on as-cast samples and heat treated samples to obtain an ADI grade 1. In both cases, we studied samples taken from two well differentiated "Y" block sizes. The results obtained show that, for the chemical composition analyzed, both castings have a fractomechanical response decrease as the temperature diminishes. Besides, the block size enlargement produce a deterioration of the mechanical properties (the fracture toughness, mainly), for both castings. |
topic |
cast iron ADI fractomechanics low temperature |
url |
http://www.scielo.br/scielo.php?script=sci_arttext&pid=S1516-14392002000200009 |
work_keys_str_mv |
AT vefierro fractomechanicalpropertiesofascastandaustemperedsgcastironbetween40cand20c AT jasikora fractomechanicalpropertiesofascastandaustemperedsgcastironbetween40cand20c AT fraguera fractomechanicalpropertiesofascastandaustemperedsgcastironbetween40cand20c AT hnalvarezvillar fractomechanicalpropertiesofascastandaustemperedsgcastironbetween40cand20c AT afansaldi fractomechanicalpropertiesofascastandaustemperedsgcastironbetween40cand20c AT pjjratto fractomechanicalpropertiesofascastandaustemperedsgcastironbetween40cand20c |
_version_ |
1725609153755348992 |