Enhanced luminescence at 2.88 and 2.04 μm from Ho3+/Yb3+ codoped low phonon energy TeO2–TiO2–La2O3 glass
The high phonon energy and short infrared cut-off wavelength of conventional oxide glass (or crystal) hosts are the limitations to achieve mid-infrared (MIR, λ≥2.5μm) luminescence. In present study, the luminescence performance of low phonon and non-conventional TeO2-TiO2-La2O3-based glass (TTL) hos...