Construction and analysis of dynamic solidification curves for non-equilibrium solidification process in lost-foam casting hypo-eutectic gray cast iron
Most lost-foam casting processes involve non-equilibrium solidification dominated by kinetic factors, while construction of a common dynamic solidification curve is based on pure thermodynamics, not applicable for analyses and research of non-equilibrium macro-solidification processes, and the const...
Main Authors: | Ming-guo Xie, Chang-an Zhu |
---|---|
Format: | Article |
Language: | English |
Published: |
Foundry Journal Agency
2017-05-01
|
Series: | China Foundry |
Subjects: | |
Online Access: | http://ff.foundryworld.com/uploadfile/2017060939951573.pdf |
Similar Items
-
Eutectic solidification mode of spheroidal graphite cast iron and graphitization
by: Hideo Nakae, et al.
Published: (2007-02-01) -
Solidification sequence and design curves for "T" shape castings /
by: Hodjat, Yahya
Published: (1981) -
Solidification Pattern of Si-Alloyed, Inoculated Ductile Cast Irons, Evaluated by Thermal Analysis
by: Iuliana Stan, et al.
Published: (2021-05-01) -
Estimation Of Cooling Rates In Suction Casting And Copper-Mould Casting Processes
by: Kozieł T.
Published: (2015-06-01) -
Microsegregation and controlled solidification of magnesium-treated cast irons.
by: Riding, Allan Lance.
Published: (1970)